Grades of materials used for..
Pipes Fittings Flanges acc. to various ASTM standards


What are ASTM Grades..

ASTM standards define the specific manufacturing process of the material and determine the exact chemical composition of pipes, fittings and flanges, through percentages of the permitted quantities of carbon, magnesium, nickel, etc., and are indicated by "Grade".

For example, a carbon steel pipe can be identified with Grade A or B, a stainless-steel pipe with Grade TP304 or Grade TP321, a carbon steel fitting with Grade WPB etc..

Below you will find as an example 3 tables with chemical requirements for..

  • Flanges ASTM A182 Grade F304, F304L F316L
  • Pipes ASTM A312 Grade TP304, TP304L, TP3016L
  • Fittings ASTM A403 Grade WP304, WP304L, WP316L

Furthermore, a table with frequently used ASTM Grades, arranged on Pipes, Fittings, Flanges, Valves, Bolts and Nuts, which belong together as a group.

As you may be have noted, in the table below, ASTM A105 has no Grade. Sometimes ASTM A105N is described;
N stands not for Grade, but for normalized. Normalizing is a type of heat treatment, applicable to ferrous metals only. The purpose of normalizing is to remove the internal stresses induced by heat treating, casting, forming etc..


Chemical requirements composition, %
Flanges ASTM A182

Grade C Mn P S Si Ni Cr Mo
F304 0.08 2 0.045 0.03 1 8 - 11 18 - 20  
F304L 0.03 2 0.045 0.03 1 8 - 13 18 - 20  
F316L 0.03 2 0.045 0.03 1 10 - 15 16 - 18 2 - 3
Note..
Grades F304, F304L, and F316L shall have a maximum Nitrogen content of 0.10%.

Chemical requirements composition, %
Pipes ASTM A312

Grade C Mn P S Si Cr Ni Mo
TP 304 0.08 2 0.045 0.03 1 18 - 20 8 - 11  
TP 304L 0.035 2 0.045 0.03 1 18 - 20 8 - 13  
TP 316L 0.035 2 0.045 0.03 1 16 - 18 10 - 14 2 - 3
Note..
For small diameter or thin walls or both, where many drawing passes are required, a Carbon maximum of 0.040% is necessary in grades TP304L and TP316L. Small outside diameter tubes are defined as those less than 0.50 in. [12.7 mm] in outside diameter and light wall tubes as those less than 0.049 in. [1.20 mm] in average wall thickness (0.044 in. [1.10 mm] in minimum wall thickness).

Chemical requirements composition, %
Fittings ASTM A403

Grade C
(1)
Mn
(1)
P
(1)
S
(1)
Si
(1)
Ni Cr Mo
WP 304 0.08 2 0.045 0.03 1 8 - 11 18 - 20  
WP 304L 0.03 (2) 2 0.045 0.03 1 8 - 12 18 - 20  
WP 316L 0.03 (2) 2 0.045 0.03 1 10 - 14 (3) 16 - 18 2 - 3
Notes..
(1) Maximum, unless otherwise indicated.
(2) For small diameter or thin walls or both, where many drawing passes are required, a Carbon maximum of 0.040% is necessary in grades TP304L and TP316L. Small outside diameter tubes are defined as those less than 0.50 in. [12.7 mm] in outside diameter and light wall tubes as those less than 0.049 in. [1.20 mm] in average wall thickness (0.044 in. [1.10 mm] in minimum wall thickness).
(3) On pierced tubing, the Nickel may be 11.0-16.0%.


Frequently used ASTM Grades

Material Pipes Fttg Flg Valves Bolts & Nuts
Carbon Steel A106 Gr A A234 Gr WPA A105 A216 Gr WCB A193 Gr B7
A194 Gr 2H
A106 Gr B A234 Gr WPB A105 A216 Gr WCB
A106 Gr C A234 Gr WPC A105 A216 Gr WCB
Carbon Steel
Alloy
High-Temp
A335 Gr P1 A234 Gr WP1 A182 Gr F1 A217 Gr WC1 A193 Gr B7
A194 Gr 2H
A335 Gr P11 A234 Gr WP11 A182 Gr F11 A217 Gr WC6
A335 Gr P12 A234 Gr WP12 A182 Gr F12 A217 Gr WC6
A335 Gr P22 A234 Gr WP22 A182 Gr F22 A217 Gr WC9
A335 Gr P5 A234 Gr WP5 A182 Gr F5 A217 Gr C5
A335 Gr P9 A234 Gr WP9 A182 Gr F9 A217 Gr C12
Carbon Steel
Alloy
Low-Temp
A333 Gr 6 A420 Gr WPL6 A350 Gr LF2 A352 Gr LCB A320 Gr L7
A194 Gr 7
A333 Gr 3 A420 Gr WPL3 A350 Gr LF3 A352 Gr LC3
Austenitic
Stainless
Steel
A312 Gr TP304 A403 Gr WP304 A182 Gr F304 A182 Gr F304 A193 Gr B8
A194 Gr 8
A312 Gr TP316 A403 Gr WP316 A182 Gr F316 A182 Gr F316
A312 Gr TP321 A403 Gr WP321 A182 Gr F321 A182 Gr F321
A312 Gr TP347 A403 Gr WP347 A182 Gr F347 A182 Gr F347


ASTM Materials

Pipes

  1. A106 This specification covers carbon steel pipe for high-temperature service.
  2. A335 This specification covers seamless ferritic alloy-steel pipe for high-temperature service.
  3. A333 This specification covers wall seamless and welded carbon and alloy steel pipe intended for use at low temperatures.
  4. A312 Standard specification for seamless, straight-seam welded, and cold worked welded austenitic stainless steel pipe intended for high-temperature and general corrosive service.

Fittings

  1. A234 This specification covers wrought carbon steel and alloy steel fittings of seamless and welded construction.
  2. A420 Standard specification for piping fittings of wrought carbon steel and alloy steel for low-temperature service.
  3. A403 Standard specification for wrought austenitic stainless steel piping fittings.

Flanges

  1. A105 This specification covers standards for forged carbon steel piping components, that is, flanges, fittings, valves, and similar parts, for use in pressure systems at ambient and higher-temperature service conditions.
  2. A182 This specification covers forged or rolled alloy and stainless steel pipe flanges, forged fittings, and valves and parts for high-temperature service.
  3. A350 This specification covers several grades of carbon and low alloy steel forged or ring-rolled flanges, forged fittings and valves for low-temperature service.

Valves

  1. A216 This specification covers carbon steel castings for valves, flanges, fittings, or other pressure-containing parts for high-temperature service and of quality suitable for assembly with other castings or wrought-steel parts by fusion welding.
  2. A217 This specification covers steel castings, martensitic stainless steel and alloys steel castings for valves, flanges, fittings, and other pressure-containing parts intended primarily for high-temperature and corrosive service.
  3. A352 This specification covers steel castings for valves, flanges, fittings, and other pressure-containing parts intended primarily for low-temperature service.
  4. A182 This specification covers forged or rolled alloy and stainless steel pipe flanges, forged fittings, and valves and parts for high-temperature service.

Bolts and Nuts

  1. A193 This specification covers alloy and stainless steel bolting material for pressure vessels, valves, flanges, and fittings for high temperature or high pressure service, or other special purpose applications.
  2. A320 Standard Specification for Alloy-Steel and Stainless Steel Bolting Materials for Low-Temperature Service.
  3. A194 Standard specification for nuts in many different material types.

Related Post(s)

ASTM logo
ASTM Material Specifications
Full list of ASME pressure and temperature ratings. Plate materials are listed only for use as blind flanges and reducing flanges without hubs. Additional plate materials listed in ASME B16.34 may also be used with corresponding B16.34, Standard Class ratings.